Abrasive Brick

显气孔率Apparent Prosity (%):≤8

密度True density g/cm3:≥3.0

抗压强度Cold Crushing Strength Mpa:≥250

线性膨胀Line Expansion 1150℃ %:0.8

Al2O3(%):71-74

Application of wear-resistant bricks: mainly used in the parts that need to use wear-resistant and high-temperature materials, such as the slide brick of the metallurgical push steel heating furnace using the steel platform (steel trough) of the stepping heating furnace (steel trough) and the lining of the waste incinerator

Product introduction of wear-resistant brick
Its compact structure, with wear resistance, impact resistance, high temperature resistance, thermal shock resistance and other advantages, mainly used in the need to use wear resistance and high temperature parts, products not only in the domestic steel began to promote the use, and has been exported to South Korea, Indonesia, Taiwan and other countries and regions.
Wear-resistant brick is made of high-quality bauxite and imported Australian zirconium sand and other raw materials, melting at high temperature in the arc furnace, casting completed, mainly used for parts that need to use wear-resistant, high temperature materials, such as the slide brick of the metallurgical push steel heating furnace using the steel platform (steel groove) of the stepping type heating furnace steel platform (steel groove) and waste incinerator lining

Specifications of wear-resistant bricks

型号Item TY-GM5
Special标准值 Typical典型值
化学指标Chemical
Composition %
Al2O3 71-74 73
ZrO2 4.5-6 5.5
SiO2 17-20 19
Na2O ≤1.0 1.0
Others ≤0.5 1.5
显气孔率Apparent Prosity (%) 5-8 <8
密度True density g/cm3 ≥3.0 3.54
抗压强度Cold Crushing Strength Mpa ≥250 350
高温耐压强度Hot Crushing Strength 1300℃ Mpa   45
线性膨胀Line Expansion 1150℃ %   0.8
导热系数Thermal conductivity 1250 ℃: W/MK   4.6
体积密度Bulk Density (g/cm3) 普通浇铸PT(RN)   ≥3.0
无缩孔浇铸WS(VF)   ≥3.2
晶相分析Crystallographic analysis % Corundum 38
Mullite 40
Glass Phase: 17
Baddeleyite 5

 

 

 

 

 

 

 

 

 